Add to Cart
Cemented Carbide Grits Carbide Broken Grain For Wear Resistance Directly From Factory Zhuzhou
1.Description of the cast tungsten carbide for welding
cast tungsten carbide Crushed are Irregular shape particles, they are in different meshes.
2, Usage of the cast tungsten carbide powder For PTA application with blending Ni or Nickel base alloy powder
Good wear resistance for oil drilling tool mineral tool.
Generate more dense coating compared with FTC, and with better hardness and wear
3.cast tungsten carbide powder physical performance
Performance chart:
Grade | Cobalt content | Binder | WC particle /grain size | Density | Hardness | Coercive force Coercivity HC | Transverse Rupture Strength Flexural strength | ||
(wt%) | (%) | (μm) | (g/cm3) | HRA | HV10 | HV30 | (KA/m) | (MPa) or (N/mm2) | |
JK09 | 10.6-12.0 | 12 | 2.4 | 14.30 | 87.30 | 1100 | 5.0-8.0 | 2900 | |
JK10.2 | 5.2-6.0 | 6 | 2.0 | 14.95 | 90.00 | 1350 | 11.2-13.0 | 2800 | |
JK10.2T | 5.4-6.0 | 6 | 2.0 | 14.95 | 90.30 | 1380 | 11.2-13.2 | 3000 | |
JK20.2 | 7.0-7.8 | 7.8 | 2.0 | 14.78 | 89.50 | 1300 | 9.2-11.3 | 3000 | |
JK10.4 | 5.0-6.0 | 6 | 4.0 | 14.94 | 87.30 | 1100 | 5.3-6.5 | 2400 | |
JK20.4 | 6.8-8.0 | 8 | 4.0 | 14.70 | 86.70 | 1050 | 4.3-5.5 | 2500 | |
JK30.4 | 8.6-10.0 | 10 | 4.0 | 14.53 | 86.30 | 1010 | 4.0-5.0 | 2600 | |
STK3050 | 8.6-10.0 | 10 | 5.0 | 14.53 | 86.30 | 1010 | 4.0-5.0 | 2650 | |
YL2 | 7.0-8.2 | 8.2 | ≤1.0 | 14.75 | 91.50 | 1530 | 17.0-19.0 | 3000 | |
YL3 | 6.8-8.2 | 8.2 | ≤1.0 | 14.70 | 91.50 | 1530 | 17.0-20.0 | 2800 | |
YL10 | 8.5-10.0 | 10 | 1.2 | 14.48 | 90.50 | 1410 | 12.5-15.5 | 3100 | |
YG6 | 14.85 | 90.00 | 2000 | ||||||
YG8E | 7.0-8.2 | 8.3 | 1.6 | 14.60 | 89.80 | 1330 | 10.0-14.0 | 2600 |
Production and test:
1)The products will start to prepare the powder as per the customer’s requirement with our wet-grinding machine
2) Before mass production, we need to do a trial pressing and sintering, and we check the appearances and the sizes of the samples with a micrometer to ensure that the requirements of the drawings can be met before batch production
3) Bulk production, press the raw materials to shape blanks, and carbide tips must be passed by semi-finished inspection.
4) Sinter blanks to finish (HIP) and finished products inspection to ensure the best quality and production capacity.